phenolic guduro don gogayya kayan
Resins don abrasives masu haɗin gwiwa sune foda da ruwa, wanda zai iya biyan buƙatun samfuran daban-daban. Wannan jerin an karɓi kayan aikin samarwa na ci gaba da sarrafawa. Tare da tsantsar ƙira, ingantaccen nauyin kwayoyin halitta da hanyar rarrabawa, yana sanya rarrabar ƙwayoyin guduro ya kai matsayi na musamman. The foda guduro yana halin da karfi danko, inji ƙarfi, abrasion juriya, zafi juriya da rigar nika kwanciyar hankali. A matsayin wakili mai kyau na wetting, resin ruwa yana da kyakkyawan aikin jika da kuma rarraba rashin daidaituwa. Yana sanya resin ruwa tare da zafi mai kyau ta hanyar aiki na musamman. A ƙarƙashin yanayin zafi mai zafi, guduro ba zai zama caking ba, kuma tare da babban ƙarfi da babban aikin niƙa, samfuri ne mai kyau wanda yawancin masana'antun injin niƙa suka zaɓa.
Bayanan fasaha don guduro foda
Daraja |
Bayyanar |
phenol kyauta (%) |
kwararar pellet / 125 ℃ (mm) |
magani /150℃(s) |
Granularity |
Aikace-aikace/ Halaye |
2123-1 |
Farar fari / haske rawaya foda |
≤2.5 |
30-45 |
50-70 |
99% karkashin 200 raga |
Babban manufar faifai ultra-bakin ciki (kore, baki) |
2123-1A |
≤2.5 |
20-30 |
50-70 |
Fayil mai ƙarfi mai ƙarfi (kore) |
||
2123-1T |
≤2.5 |
20-30 |
50-70 |
Faifai mai ƙarfi mai ƙarfi (baƙi) |
||
2123-2T |
≤2.5 |
25-35 |
60-80 |
Ƙarfin niƙa/yanke dabaran (gyara) |
||
2123-3 |
≤2.5 |
30-40 |
65-90 |
Dabarun yankan ƙarfi mai ƙarfi (nau'i mai ɗorewa) |
||
2123-4 |
≤2.5 |
30-40 |
60-80 |
Ƙaddamar da dabaran niƙa (nau'i mai dorewa) |
||
2123-4M |
≤2.5 |
25-35 |
60-80 |
Dabarar niƙa ta musamman (nau'in kaifi) |
||
2123-5 |
≤2.5 |
45-55 |
70-90 |
Niƙa dabaran lafiya kayan sadaukar |
||
Saukewa: 2123W-1 |
Farin fari/mai haske rawaya |
3-5 |
40-80 |
50-90 |
– |
rigar raga |
Bayanan fasaha don guduro ruwa
Daraja |
Danko / 25 ℃ (cp) |
SRY(%) |
phenol kyauta (%) |
Aikace-aikace/Halayen |
213-2 |
600-1500 |
70-76 |
6-12 |
rigar raga |
2127-1 |
650-2000 |
72-80 |
10-14 |
mai kyau rigar iyawa |
2127-2 |
600-2000 |
72-76 |
10-15 |
High ƙarfi mai kyau rigar iyawa |
2127-3 |
600-1200 |
74-78 |
16-18 |
Kyakkyawan anti-attenuation |
Shiryawa da ajiya
Flake / Foda: 20 kg / jaka, 25kg / jaka, Resin ya kamata a adana shi a wuri mai sanyi, bushe da iska mai kyau. Rayuwar ajiya shine watanni 4-6 a ƙasa 20 ℃. Launinsa zai zama duhu tare da lokacin ajiya, wanda ba zai yi tasiri a kan darajar resin ba.